I've always secretly hoped for this but was concerned if that would be classified as hazardous material during shipping.
I have a friend interested in making PURE retr0brite- the issue is, one of the ingredients (found in the oxy booster), if bought locally or over the counter leaves behind a white residue that damages the case.
So, he looking into buying the certain component that actually is used and doesn't leave residue- but you have to buy it in massive amounts.
It is possible but someone would have to get a kickstarter thing going to raise initial money to get off the ground.
Which, to me sounds interesting and if I wasn't going into a difficult faculty for University I would probably try it out. If I switch to arts second year, I'll do this (assuming nobody else does)
Look, high concentrations of hydrogen peroxide is impractical.
1. Explosive risks and risk to flesh
2. Anything over 35% need homeland security background check to buy.
3. Hazardous materials handling fees when shipping.
If you are curious try the legal limit in us 17% peroxide and ammonia (do it outdoors) and let it fully oxidize.
Actually I've heard it's better to use 40 volume clear developer and just submerge whatever you want whitened into it. The main beef I have with Retr0bright is that it's non-uniform and it can create splotches if it's not spread well enough.
Retrobrite is more likely some form of slower acting more powerful oxidizer.
Hydrogen peroxide exhausts fast, with heat.
I am betting retrobrite has a good portion of common tooth bleaching oxidizer in it; carbamide peroxide which would explain
the uneven color changes.
The science is in the link, if you actually want to know what it does.
It does work, I have first hand experience. Brightened up an old Macintosh SE/30.
It's only uneven if you apply it unevenly and don't expose it properly to UV light- the sun works but you need to rotate it. If you've got a UV bulb, that produces some serious results.
I used lab quality 45%, and it was done quickly. Done a second time with 10%- more patience required but otherwise same results
I'm not sure that a "mass-produced" Retr0bright would even be useful, since you still need to add the oxy action to get the reaction going.
If you're after an easy way to Retr0bright, I'd recommend using a hydrogen peroxide creme from a hair salon. It comes already thickened, so all you need to add is the oxy action. This is pretty much the only option for me, since I can't find any stores in Australia that sell big bottles of straight hydrogen peroxide, in order to submerge the item. Even buying a whole bunch of small bottles is still really expensive.
The point of the gel method is to avoid having to submerge something. That seriously reduces the amount of HOOH you need.
One advantage of using lower concentrations is that it slows the reaction down. That may seem odd, but the reaction still does produce heat. If you live in a hotter climate--especially if you're using direct sunlight--a slower reaction can prevent plastic from heat warping.
Cool! Thanks for posting. I'll probably pick some up and give it a try!
might have to swing by a Sally's
It's not just exclusive to your US Sally chain (I mean they didn't invent it). We've got it in Poland as well, here it's known as Scandic oxydant 12% (roughly the equivalent to volume 40)